High Chrome Seat

• 18-22% Chromium for resistance to abrasion, corrosion and deformation
• 1-2% Nickel content, which lends corrosion-resistance and toughness
• Machined from solid bar stock and ground to exacting tolerances
• The alternative to Powder Metal
• Machines as a continuous chip
• Use KPMI® “High Chromium Seats” for your next gasoline or diesel engine rebuild